Joint bulk melt textured superconducting TrBa2Cu3O7 tiles where Tr is rare earth or YTRIUM, and welding procedure based on Ag tape agent.
Inventors: Teresa Puig Molina; Xavier Obradors Berenguer; Simona Iliescu; Xavier Granados García; Ana Esther Carrillo Fernández; Elena Bartolomé Porcar
Name: Joint bulk melt textured superconducting TrBa2Cu3O7 tiles where Tr is rare earth or YTRIUM, and welding procedure based on Ag tape agent.
Application number: 200300081
Patent number: ES2212751
Priority country: Spain
Date: 14/01/2003
Conferral date: 12/09/2005
Holding institution: Consejo Superior de Investigaciones Científicas